wahyu.wb29
Quiz by , created more than 1 year ago

EXAM Preparation for API 510

915
1
0
No tags specified
wahyu.wb29
Created by wahyu.wb29 almost 9 years ago
Close

API 510 OPEN BOOK

Question 1 of 5

1

1. When making repairs to stainless-steel overlay on carbon steel base material, the repair shall be inspected by ?

Select one of the following:

  • A. Radiographic testing

  • B. Penetrant testing

  • C. Ultrasonic examination

  • D. Penetrant and ultrasonic testing

Explanation

Question 2 of 5

1

2. Temper embrittlement is a metallurgical change that is ?

Select one of the following:

  • A. Not readily apparent but can be confirmed through tension testing

  • B. Readily apparent and can be confirmed through impact testing

  • C. Readily apparent and can be confirmed through metallography

  • D. Not readily apparent but can be confirmed through impact testing

Explanation

Question 3 of 5

1

3. Non – normalized SA 516 Gr 60 material is used for fabricating a pressure vessel that has a nominal wall thickness of 1.125 inches (28.6mm). What is the minimum design metal temperature for the vessel that does not require impact testing ?

Select one of the following:

  • A. - 26˚F (-32˚C)

  • B. 2˚F (-17˚C)

  • C. 37˚F (3˚C)

  • D. 75˚F (24˚C)

Explanation

Question 4 of 5

1

4. When reviewing a group of radiographs, all following information must be documented except ?

Select one of the following:

  • A. Source to object distance

  • B. Geometric un sharpness

  • C. Material type

  • D. Single or double wall exposure

Explanation

Question 5 of 5

1

5. If a repair is made on a pressure vessel using a filler metal with lower specified minimum tensile strength than base metal, all of the following requirement apply except ?

Select one of the following:

  • A. The repair shall be made with minimum of two passes

  • B. The increased thickness of the repair shall have rounded corners and blend into the base metal using a 3 : 1 taper

  • C. A minimum preheat of 175 Deg F (79.4 Deg C) and an inter pass temperature of 450 Deg F (232Deg C)must be maintained

  • D. The repair thickness shall not more than 50 % of the required base metal thickness excluding corrosion allowance

Explanation