Cupping When timber bends across the grain. Annual rings can be clearly seen on the end of the wood and the varying length of them means the wood dries at different speeds. This means the wood shrinks at different rates and cups.
Twisting Can twist as it dries if the wood has come from the centre of a tree and has a spiral grain. Normally unusable.
Splitting Where the grain separates at the end of a piece of wood - only thing to do is cut the affected ends off.
Knots Natural by-product of where branches were attached to the tree. Can become loose and drop out if dead - which is very dangerous if the wood is being machined. Can be tight however, and even then are still a nuisance in terms of working the wood. Softwoods like pine tend to have many more knots.
Mostrar resumen completo Ocultar resumen completo

Similar

Material Processing and Forming
Alec Stevens
CAD/CAM
Alec Stevens
Mechanical, Heat and Chemical Joining Techniques
Alec Stevens
Material Removal
Alec Stevens
Heat Treatments
Alec Stevens
Modelling and Prototyping
Alec Stevens
Wood Conversion and Seasoning
Alec Stevens
Techniques for Mass Production
Alec Stevens
Scale of Production
Alec Stevens
GCSE Revision (Plastics detailed) AQA specification
T Andrews
Plastics
fampulli