- 1polymers response to an applied stress or strain depends uponthe rate or time period of loading
- 2At low temperatures and high rates of strain polymers displaydisplay elastic behavior
- 3at high temperatures and low rates of strain polymers behavethey behave in a viscous manner, flowing like a liquid
- 4viscoelasticthey display aspects of both viscous and elastic types of behaviour.
- 5stress σequal to force over area of applied force
σ =F/A - 6strain emeasure of how much a shape changed
e=change in shape/initial shape - 7describe creep loadinga constant stress is applied to the specimen at t = 0 and the strain increases rapidly at first, slowing down over longer periods of time. In an elastic solid, the strain stays constant with time.
- 8stress relaxationthe strain is held constant and the stress decays slowly with time, whereas in an elastic solid it would remain constant.
- 9describe a tensile testa polymer is set in a dog bone shaped mold, and is clamped into a machine at the ends, the machine pulls the bone both ways to stretch out the mold. The force applied and the change in shape are measured, which can be converted to a stress v strain plot
- 10rates of strain are between1-100% per minute
- 11at higher rates of strain, the tensile strength and modulus aref(strain rate), a function of strain rate
- 12at higher strain rates, the temp of the sample mayincrease, complicating the measurement
- 131 psi = ? Pa6895 Pa
- 14equation of stress v strain plot w modulusstress= Modulus*strain
σ =Ee - 15Boltzmann superposition principleIt allows the state of stress or strain in a viscoelastic body to be determined from knowledge of its entire deformation history.
- 16—A. elastic behavior, deformation is recoverable, due to bending and stretching of interatomic bonds, slope is young's modulus
B. yield at stress, elastic limit, deformation is no longer recoverable after B
C. deformation of the molecular structure of the polymer, chains slide
D. necking region, or cold drawing, ploymer mold stretches, only happens at cold temps
E. strain hardening region, polymer chains align to form crystals
F. ultimate strength, strength at break
- 17—


- 18—describe the molecular structure changes along the plot

- 19necking region/ cold drawingthe polymer mold is stretched as the polymer chains with the mold are straightened out and untangled, stress is absorbed as this happens, only occurs at low temp
- 20youngs modulusE=stress/strain
slope of the initaial linear part of the stress v strain plot, below the proportional limit - 21secant modulusratio of total stress to corresponding strain on stress-strain curve, not always linear

- 22nominal or engineering stress/strainwhen measuring stress, you measure the force over the initial area, as strain increases, the initial area changes, we still measure the force over the initial area bc true stress is hard to measure
- 23elastic regionwhere the polymer is strained by can still go back to its initial shape
- 24strain hardeningstrain hardening is when the material becomes stronger as the stress increases. Occurs when the initial orientation of the polymer is random, and the stress pulls the chains into a crystalline structure
- 25soft materials willhave low modulus, are easily deformed at low stress
- 26weak material willbreak and bends at low stress
- 27draw a soft, weak stress-strain curveex. teflon
low modulus, low yeild strength, low ultimate strength
- 28yield strengthcan be defined as the onset of permanent plastic deformation in a material which is not recovered when the stress is removed.
- 29hardhigh modulus, material will not deform until high stress
- 30brittlevery little plastic deformation, no necking or hardening
- 31hard brittle stress-strain curve

- 32toughnessability of a material to absorb energy before breaking, tough polymers will have a large area under the stress-strain curve
- 33soft tough stess-strain curve

- 34strong materialmaterial can resist heavy impact; resist both deformation and failure
- 35hard strong curve

- 36hard tough curve

- 37tensile strength is the same asstress at break
- 38why is polycarbonate (hard tough) used for plexi glassthe material has a high modulus and doesn't not deform until high stress, and the toughness allows for the material to absorb so energy before breaking, its cracks and doesn't shatter
- 39a slower rate of strain givesmore stretching/ hardening, large deformation region, chains can slowly disentangle from one another and align
- 40a higher rate of strain givesa high young's modulus, but no deformation region, no time for chains to rearrange and they break
- 41rate effects: as the modulus increases the,yield strength increases
- 42rate effects: increasing the rate of strain is the same asdecreasing the temperature
- 43work to rupturethe area under the stress-strain curve, a method to measure toughness
- 44rate effects: as the rate of strain increases, the elongation at break __decreases, less time for the polymer chains to rearrange and deform, so mold just breaks
- 45rate effects: as the rate of strain increases, the area under the curvedecreases, the toughness of the material is decreasing, to brittle
- 46rate effects: raising the temp of a test will cause the yield point todecrease, as well as the youngs modulus
- 47ductile to brittle transitiontemp at which a polymer does not draw and behaves more brittle, occurs around Tg
- 48time- temp superpositionthe effect of changing temp or rate of strain of a test to change the stress-strain curve.
increasing rate of strain, or decreasing temp, makes polymer behave more brittle, - 49elastomercan return to original shape after a stress is applied and released.
elastomer stress-strain curves have no yield point - 50stress relaxation-elongate the sample to a certain strain, monitor stress as a function of time
- 51describe hysteresis graph

- 52creep experimentconstant stress is applied and maintained while strain is measured over time
- 53describe hysteresisThe elastomer will return to its original state after stretching, but absorbs a lot of energy (area in circle), so will only stretch 1-2 times before deformation
the energy in form of heat is formed by friction of the polymer chains as they are pulled, polymer becomes less elastic over time - 54chain stiffness effectschain stiffness (side groups) make it harder for chains to slide, decreases deformation area, increase yield point and Tg
- 55which is stronger, crystalline polymer or amorphous polymer of same structurecrystalline
- 56stronger amorphous polymers have ahigher Tg
- 57Izod and charpy impact tests measuretoughness, ability to absorb energy, measures energy to cause a rupture
- 58energy required to break sample is proportional tothe difference in hight before and after the test
- 59formula for impact strengthimpact strength = energy to break per unit thickness= (H1-H2)*Weight of hammer*(1/width of sample)
- 60describe izod test

- 61describe charpy test

- 62important variables of izod testing1. size of sample mold
2. method of notching
3. speed of notching tools
4. quality of notch
5. time between notching and test
6. thickness
7. environmental conditions - 63rate effects: increasing the temp causes the time to deformation todecrease
- 64Williams Landel Ferry equation

- 65—
Informationen
- Beschreibung
- polymer chem Karteikarten am Chapter 20 and mechanical properties, erstellt von Ashlin Deatherage am 27/11/2022.
- Erstellt von
- Ashlin Deatherage
- Aufrufe
- 2
- Bewertung