Flashcards
Welding Defects and Discon

Flashcards do conjunto (24)
- 1True or False Incorrect weld profile is a weld that does not meet the requirements for size and contour.TRUE
- 2What is Overlap?Overlap is the bulging or protruding portion of a weld that extends beyond the toe, face, root.

- 3( Blank is a weld face or root that is depressed or extends below the adjacent base metal surfaces.Insufficient throat or Underfill

- 4( Blank) is a groove melted into the base metal adjacent to the toe or root of a weldUndercut

- 5Excessive ( Blank ) is a type of contour formed by excessive reinforcement.Convexity

- 6( Blank ) and ( Blank ) are caused by the nonuniform expansion and contraction of the weld and base metal during the heating and cooling process of welding.Distortion and Warpage

- 7Internal Inconsistencies or IrregularitiesCracks
Porosity
Slag
Inclusions
Incomplete fusion
Inadequate Joint Penetration - 8( Blank ) are fractures that cause an opening or a split in the weld or base metalCRACK

- 9A ( Blank ) crack runs along parallel to the axis of the weldLongitudinal Crack

- 10A ( Blank ) crack runs perpendicular to the axis of the weld.Transverse Crack

- 11( Blank ) cracks occur in the depression left at the termination of the weld bead.Crater Cracks

- 12( Blank ) are longitudinal in the weld and originate from the face or rootWeld Metal Cracks

- 13( Blank ) cracks originate and grow from the toe of the weld where high amounts of stress are most commonToe Cracks

- 14( Blank ) cracks are located along the root of the weldRoot

- 15( Blank ) strike is a heat-affected surface, any localized remelted surface, or change in surface profile caused by the arcArc Strick

- 16( Blank ) or underbead cracks occur during the cooling cycle after solidification of the weld and normally do not extend to the surface of the weldment.Heat-Affected Zone Cracks

- 17You guys are doing great!!!

- 18( Blank ) is entrapped gas cavities formed during solidification of the weldPorosity

- 19( Blank ) porosity is found in groups at specific pointsClustered Porosity
- 20( Blank ) porosity generally follows a line parallel to the axis of the weldLinear Porosity

- 21( Blank ) or worm holes or blow holes, appear as a cylindrical cavity.Piping

- 22( Blank ) are nonmetallic solid material trapped within the weld metal or between the weld and base metal during solidification.Slag Inclusions

- 23( Blank ) fusion is the failure of the liquid weld metal to flow into and fuse the total face area of the joint.Incomplete