143. When making repairs to a stainless steel cladding, the base metal should be checked for
delayed cracking when the base material is:- AA. P1 or P3.
- BB. P1 thru P11.
- CC. P1, P3, P4 or P5.
- DD. P3, P4, or P5.
246. A welded repair is made to stainless steel cladding. The vessel's base material is carbon
steel. The completed weld repair should be examined using:- AA. MT
- BB. PT
- CC. MT or PT
- DD. MT and UT (flaw detection)
- EE. PT and UT (flaw detection).
- FF. MT or PT, and UT (flaw detection).
347. A welded repair is made to stainless steel cladding. The vessel's base material is a P-4
steel. The completed weld repair should be examined using:- AA. MT
- BB. PT
- CC. MT or PT
- DD. MT and UT (flaw detection)
- EE. PT and UT (flaw detection)
- FF. MT or PT, and UT (flaw detection).
448. A vessel with P-5 base material is clad with stainless steel. During the turnaround,
welded repairs are made to the cladding. UT flaw detection of the repair area:- AA. is not required
- BB. must be done before welding is performed.
- CC. must be done immediately after welding is completed
- DD. must be done, but after waiting 24 hours.
- EE. must be done, by a technician certified to EPRI
560. During a vessel repair or alteration, when can preheating be used as an alternative for
postweld heat treating?- AA. For P 1 & P3 materials
- BB. For Pl, P3 & P4 materials
- CC. For P3, P4 and P5 materials
- DD. For P1 through Pll materials
- EE. Whenever the inspector reviews and approves the procedure
664. During a vessel repair or alteration, when can controlled deposition welding be used as an
alternative for postweld heat treating?- AA. For PI & P3 materials
- BB. For Pl, P3 & P4 materials
- CC. For P3, P4 and P5 materials
- DD. For Pl through Pll materials
765. Welding is performed on an in-service vessel. What welding processes can be used when
using controlled deposition welding as a substitute for postweld heat treating?- AA. Only SMAW
- BB. Only SMAW and SAW
- CC. Only SMAW and GMAW
- DD. Only SMAW and GTA W
- EE. Only SMAW, GMAW and GTAW
- FF. Only SMAW, SAW, GMAW and GTAW
- GG. Any welding process provided the engineer approves
861. Welding is performed on an in-service vessel. What welding processes can be used when
using preheat as a substitute for postweld heat treating?- AA. Only SMAW
- BB. Only SMAW and SAW
- CC. Only SMAW and GMAW
- DD. Only SMAW and GTAW
- EE. Only SMAW, GMAW and GTAW
- FF. Only SMAW, SAW, GMAW and GTAW
- GG. Any welding process provided the engineer approves
969. A corroded area in a carbon steel vessel is being repaired by using weld overlay (weld
build-up). The vessel surface should be examined by:- AA. MT or PT before welding.
- BB. MT or PT after welding.
- CC. MT or PT both before and after welding.
- DD. MT or PT after welding, and UT flaw detection after 24 hr
- EE. MT or PT both before and after welding, and UT flaw detection after 24 hrs
Information
- Description
- Quiz on V102209 CL 8/5 PUTAR PUTAR CHERABDAY, created by Wan Din on 22/09/2021.