Ajude a dar forma ao GoConqr. O que a gente deve adicionar?

Flashcards

MEEN 360 Midterm Exam Study

Daniel Varnau Engineering Inglês 76 flashcards

Stress-Strain Curve

Flashcards do conjunto (76)

  1. 1StrengthMax stress before yield/fracture
  2. 2StiffnessResistance to deformation elastically
  3. 3DuctilityAbility to plastically deform significantly before rupture
  4. 4ToughnessEnergy absorbed before fracture (Tensile/Impact/Fracture)
    Energy absorbed before yield (Modulus of resilience)
  5. 5HardnessResistance to permanent deformation (scratch, dent)
  6. 6Fatigue ResistanceResistance to fracture under cyclic load
  7. 7Creep ResistanceResistance to plastic deformation under long-term stress
  8. 8Yield StrengthThe point where the material transitions from elastic to plastic deformation (obtained from tensile test)
  9. 9Modulus of ResilienceThe elastic energy a material can absorb prior to yielding
    Er = 1/2(yield strength)(strain at yielding)
  10. 10Stress-Strain CurveStress-Strain Curve
  11. 11Work Hardening Exponent (n)Work Hardening Exponent (n)
  12. 12Ductile vs Brittle FractureDuctile vs Brittle Fracture
  13. 13Temperature Effect on Ductile Metal-Modulus of elasticity: E does not change
    -Yield strength: As temp increases, Sy decreases (due to dislocation movement)
    -Tensile (ultimate) strength: As temp increases, Sut decreases (due to dislocation density)
    -Tensile Toughness: As temp increases, U increases
  14. 14Ductile-Brittle TransitionBCC material transitions from brittle to ductile at this temp
  15. 15Hardness Measurement TechniquesTesting: Brinell, Rockwell, Microhardness, and nanoindentation
    Benefits: inexpensive, nondestructive, can be used to estimate other mechanical properties (tensile strength)
  16. 16Fracture Toughness (Kc)Material property
    Stress intensity factor required for crack to propagate
    Higher Kc means less crack propagation, more energy absorption
    Factors improve Kc - How?
    -Ability to deform (ductility). e.g. higher temp
    -Potentially smaller grain size? Crack needs more energy to propagate through one grain to next grain
    -Lower dislocation density (ductility inc.)
  17. 17Modes of FractureModes of Fracture
  18. 18Ductile Fracture1. Proceeds relatively slowly
    2. Extensive plastic deformation
    3. Stable crack
    4. Require more strain energy
    5. Easier to see the warning
    6. Most metals/some polymers (T > Tg)
    7. Cup-and-cone fracture surface
  19. 19Brittle Fracture1. Cracks may spread rapidly
    2. Little plastic deformation
    3. Unstable crack
    4. Less strain energy
    5. Occurs suddenly without warning
    6. Ceramics/some metals/some polymers (T < Tg)
    7. Fracture surface perpendicular to the direction of the applied stress
    8. Relatively flat, bright, smooth, fracture surface
    9. Chevron patterns (V-shaped markings) due to crack propagates from the origin at different levels
  20. 20Weibull StatisticsProbability of fracture vs. applied stress
    Brittle fracture uses Weibull Distribution
    Any stress > 0 in brittle material is possible to cause fracture
    Weibull modulus (m) - slope of Weibull plot
    Characteristic Strength (sigma_0) - ln(sigma0) is the x-intercept of Weibull plot
  21. 21FatigueThe lowering of strength of failure of a material due to repetitive stress which may be above or below the yield strength
    N - # of cycles to failure
    S - typical amplitude of stress (sigma_a)
  22. 22Crack Growth Rate1. Below threshold delK, crack will not grow
    delKth = Kop - Kmin
    2. Slow growth
    3. Power Law
    da/dN = C(delK)^n
    4. Rapid growth (unstable)
    Kmax > KIC
  23. 23Improve Fatigue LifeMost cracks leading to the fatigue failure originate at surface position especially at stress concentration site
    -Reduce stress concentration in design
    -Surface treatment
  24. 24CreepTime dependent deformation under constant stress (below yield strength, typically at higher temp)
    The time required for failure is the rupture time
    The creep rate and rupture time (tr) follows an Arrhenius relationship
  25. 25PolymerizationChemically join small molecules (monomer - one unit, or oligomers - a few units) to form giant molecules
  26. 26Polymer ArchitectureAffect density, strength, viscosity, solubility, glass transition temperature (Tg)
    Increasing Strength: Linear, Branched, Cross-Linked, Network
  27. 27ThermoplasticsLinear or branched molecules
    Weak Van der Waals between chains
    Low Tg and melt (Tm) upon heating
    Easy to recycle e.g. Polyethylene (PE)
  28. 28ThermosetsHighly cross-linked or 3D network structure
    Stronger but more brittle than thermoplastics
    High Tg, decompose at high T (no Tm)
    Hard to recycle e.g. Polyurethane (PU)
  29. 29Addition PolymerizationFree radical polymerization
    By broken unsaturated double bond (by T, P, catalyst)
  30. 30Condensation PolymerizationA small molecule (water, ethanol, methanol, etc.) forms during condensation polymerization
  31. 31Degree of PolymerizationNumber of repeat units
    (Average molecular weight of polymer) / (Molecular weight of repeat unit)
  32. 32TacticityDistribution or arrangement of non-symmetrical repeat unit (atoms or atomic groups)
    -Isotactic: atoms are all on the same side
    -Syndiotactic: atoms generally occupy positions on opposite side of chains
    -Atactic: random arrangement of atoms (poor packing, low density, low strength, poor resistance to heat or chemical attack)
  33. 33CopolymersContains 2 or more types of monomersCopolymers
  34. 34Temperature Effects on PolymersDepends on whether the polymer is easy to crystallize and cooling rate
    -Rubbery and leathery state: Tm>T>Tg, under stress => elastic and plastic deformation
    -Glassy state: Hard, rigid, brittle, T
  35. 35Crystallinity in PolymersPolymers are never 100% crystalline. They are semicrystalline material consists of crystalline regions and amorphous regions
    Crystallinity affect physical, chemical and optical properties
    -Higher crystallinity => denser, stiffer, harder, tougher and more resistant to solvents
  36. 36Mechanical Properties of ThermoplasticsMostly non-newtonian, viscoelastic behavior
    Elastic behavior:
    -Distort segments of polymer chains: Recovery over a long period of time => viscoelastic elastic deformation
    -Stretch and distort covalent bonds => elongate chain elastically: Recovery is instantaneous
  37. 37Plastic Deformation of ThermoplasticsStress drop beyond yield pt
    Chain will stretch, rotate, slide or disentangle
    Necking: continued sliding of the chains in necking region
    When chains are nearly parallel:
    -van der Waals force lined up
    -need greater stress to deform
  38. 38Viscoelastic CreepThermoplastics exhibit creep, a time dependent permanent deformation with constant stress or load
    Due to movement of chains (vs. diffusion in metal)
  39. 39Stress RelaxationStress decreases with time at constant strain
    Relaxation occurs more rapidly at higher T
  40. 40CrazingOccurs in thermoplastics when localized regions of plastic deformation occur in a direction perpendicular to that of the applied stress
  41. 41BlushingRefers to failure of a plastic because of localized crystallization (due to repeated bending, for example) that ultimately causes voids to deform
  42. 42ElastomersCoil like deformation, large elastic deformation > 200%
    Can be thermosets or thermoplastics
    Prevent viscous plastic deformation while retaining large elastic deformation by cross-linking the chains
  43. 43Cold WorkingThe application of a stress higher than yield strength to a metal, deforming it and increasing strength by leaving a residual strain
    Effective in simultaneously shaping and strengthening metals at the expense of reducing ductility
    At low T, deform and strengthen the material at same time
    Manufacturing Processes: forging-open die, rolling, extrusion, forging-closed die, stamping, wire drawing
  44. 44Strain Hardening Exponent (n)higher n, higher yield strength, work hardening effect is stronger
  45. 45Strain Rate Sensitivity (m)Describes how the flow stress changes with strain rate
    It is useful for predicting high-impact behavior of a material
    Typically m < 0.1 for metals and increases with temperature
    In general, higher values of m and n can resist necking => better formability
  46. 46SpringbackThe elastic strain that is recovered after a material has been plastically deformed
    It is important in the processing of polymers by extrusion and shaping automotive body panels from sheet steel
  47. 47Bauschinger EffectThe effect in which a material which has been plastically deformed under a tensile stress shows a reduction in compressive strength, and vice versa
  48. 48Strain Hardening MechanismsDuring plastic deformation of metals, dislocations density increases
    Eventually dislocations interfere with their own motion, increasing strength
  49. 49Little to No Strain Hardening in Certain Materials-Ceramics
    *Can have some small strain hardening
    *Dislocations are not very mobile and porosity (Cold working not usually possible)
    -Silicon
    *Too brittle to strain harden appreciably
    -Glasses
    *Amorphous => no dislocations => no strain hardening
    *residual stress caused by cooling rate difference: Tempered glass (compressive stress)
    *Annealed glass (no or little stress)
  50. 50Strengthening in Polymers (Thermoplastics)Strengthen upon deformation
    -Alignment and/or crystallization of polymer chains
  51. 51Properties vs. Percent Cold WorkStrain hardening controlled by the amount of plastic deformation, defined by the % CW
    % CW inc., yield and tensile strengths inc., ductility dec.
  52. 52Anisotropy From Sheet TextureDuring rolling, grains rotate and elongate, causing certain crystal directions/planes to become aligned in rolling direction
  53. 53AnnealingCan remove effects of cold working
    -Low T: eliminate residual stresses but maintain mech. prop.
    -High T: can reverse strain hardening
    Three Stages:
    1. Recovery (Removes residual stress)
    -Thermal energy permits dislocations to move and reduce residual stress
    -Form polygonised subgrains
    -Dislocation density remains the same (or similar)
    -Also called stress-relief annealing
    2. Recrystallization (dec. strength, inc. ductility)
    -New and small grains form, dislocations vanish
    -New grains tend to grow on the dislocation created polygons
    -Recrystallization temperature is not a fixed temperature
    3. Grain growth (Hall-Petch dec. yield strength)
    -Big grains grow by consuming smaller surrounding ones
    -Driven by reduction of grain boundaries
    -Strength decreases with reduced grain boundaries (big grains)
  54. 54Recrystallization TemperatureTr decreases as % CW increases
    Smaller grain size, lower the Tr
    Tr of pure metals is lower than that of alloys
    Increasing the annealing time reduces Tr
    For most of metals (in Kelvin): Tr ~ 0.4Tm
    Tr is a boundary between cold and hot working temperatures
  55. 55Hot WorkingPlastically deforming above Tr
    Almost unlimited deformation
    No strengthening
    -Recrystallization simultaneously
    Pros:
    -easier to shape (less force required)
    -eliminate imperfections (eg. dislocations, gas pores)
    Pro or Con:
    -Anisotropic behavior due to different cool rates
    Cons:
    -Poor surface finish and dimensional accuracy (oxidation of the surface, difficult to control dimensions)
  56. 56Selection of Materials Processing*Cold Working
    -We can increase the maximum deformation of a material by doing a series of cold working and subsequent annealing until the desired dimensions are reached
    *Hot Working
    -When a material is for high temperature service, recrystallization immediately causes catastrophic decrease in strength
    -Too many cycles using cold working
  57. 57NucleationFormation of secondary phase from a primary phase
    In solidification: formation of first nanocrystallites from molten metal
  58. 58Critical Radius (r*)Radius above which particle growth is accompanied by a decrease in free energy (spontaneous)
  59. 59del G*Energy required to form a stable nucleus (i.e. from an infinitely small particle)
  60. 60Critical Size for NucleationWhen Tm - T increases, r* decreases
    Undercooling: Tm - T
    del Gv increases, del G* decreases, required less energy to form a stable nucleus
  61. 61Heterogeneous NucleationHeterogeneous nucleate sites:
    -Impurities in the liquid
    -Wall of container
    Less undercooling is needed
    r* is the same. To form the curvature of a radius of r*, it requires much less atoms in the nucleus (the spherical cap)
  62. 62Hetero- vs. Homogeneous eneous NucleationHomogeneous needs large undercooling to form stable nuclei
    *Almost never occurs in liquids
    Heterogeneous requires less undercooling
    *On preexisting surfaces (e.g. Dust particles, Secondary phase particles, Mold walls and cracks)
    r* depends on T (r*hom = r*het)
    delG*hom > delG*het
    delG*het depends on delT and theta
  63. 63Controlled Nucleation-Inoculation: Adding small particles to promote nucleation => smaller grains and higher strength (e.g. adding Ti, B into Al alloy, forming Al3Ti and TiB2 serve as sites of nucleation
    -Dispersion strengthening: Form an ultra precipitates (second phase) through solid state transformations => higher strength
    -Metallic glasses: fast cooling to prevent nucleation of crystallization
  64. 64Growth Mechanisms of Planar GrowthThe manner of the growth of solid nuclei depends on how heat is removed
    Well-inoculated => heterogeneous nucleation (start from wall/impurities) => no need for undercooling
    Temp in liquid ahead of front is greater than Tm
    Removes heat from the liquid-solid interface via conduction
    -The formation of protuberance decrease temperature difference between interface and nearby solid, heat dissipation is harder, growth slow down
    -The remainder of the interface catches up
  65. 65Growth Mechanisms of Dendritic GrowthNot well-inoculated => need undercooling in liquid
    Temp in liquid ahead of front is smaller than Tm
    Dissipate heat to the liquid ahead
    -Proceeds until the liquid is not undercooled any more => planar growth
    -Only a small fraction of the total growth in pure metals
  66. 66Solidification Time (Casting)Chvorinov's Rule is a mathematical relationship that relates the solidification time for a simple casting to the volume and surface area
    V - Volume of casting (larger volume means more heat to dissipate)
    B - Mold constant, depending on casting conditions, e.g., heat of fusion, initial temperatures, heat capacity of mold, etc.
    A - Surface area in contact with mold - heat is transferred from the casted material to the mold through this area
  67. 67Secondary Dendrite ArmCooling rate inc., heat dissipating rate Q' inc., finer dendritic network (more efficient conductor of latent heat), Secondary Dendrite Arm Spacing (SDAS) dec.
  68. 68Cooling CurvesDuring solidification 2 types of heat must be removed:
    -latent heat of fusion
    -specific heat
  69. 69Casting MicrostructuresMultiple morphologies:
    -Columnar grains (anisotropic properties)
    -Equiaxed grains (isotropic properties)
  70. 70Solidification Defects - ShrinkageShrinkage (reduction in volume during solidification for most materials)
    Interdendritic Shrinkage (Micro-porosity)
  71. 71Solidification Defects - Gas PorositySolubility of gas in molten materials is relatively large
    Solubility decreases upon solidifying
    -Forms bubbles that can be trapped in solid
    To prevent:
    -Add materials to liquid that combine with the gas to form a solid
    -Ensure the partial pressure of the gas remains low
  72. 72Casting Techniques1. Sand Casting
    -Mold: green sand (water/clay/sand) or ceramics
    -Problem: cavity
    2. Investment Casting
    -Ceramic mold coated on wax
    -Lost wax process: wax removed for casting
    -Pros: complex shape
    -Appl: golf club head, bioimplants, turbine blades
    3. Permanent Mold Casting
    -Pros: Good surface, dimensional accuracy, rapid solidification, high strength, reusability
    -Cons: high cost, limited complexity in shapes
    4. Pressure Die Casting
    -Pros: Smooth, high quality surface, dimensional accuracy
    -Cons: high cost
  73. 73Ingot CastingCasting steel in molds; smaller quantity
    Non ferrous metals (Zn, Cu)
  74. 74Continuous CastingFrom molten liquid metal directly to semi-finished shape
    Cost effective for steels, Al alloys
  75. 75Directional Solidification: Single CrystalConventional - equiaxed grains
    -Problems: transverse failure along GBs
    Directional - multiple grains with GBs align along growth direction
    Single Crystal - even better for turbine blade
  76. 76Joining of Metallic MaterialsBrazing - joining metals with fillers (Tm or filler > 450 C)
    Soldering - Tm or filler < 450 C
    Characteristics of brazing/soldering
    -Metals being joined do not melt
    -Filler melt
    -Filler material is different from base material
    Fusion Welding
    -Metals being joined also melt
    -Fusion Zone (FZ), Heat Affected Zone (HAZ)
    -Fast cooling can help refine grains in FZ
    *Arc welding, laser welding, friction stir welding

Informações

Descrição
Engineering FlashCards sobre MEEN 360 Midterm Exam Study, criado por Daniel Varnau em 01-03-2024.
Criado por
Daniel Varnau
Visualizações
6
Avaliação

Fale Conosco

Sobre o que é sua mensagem?